Contents
Crushers
INTRODUCTION
1- The purpose of the preparatory processing of the raw materials is to convert theses chemically and mineralogical different materials, into raw meal of homogeneous composition. This has to be accomplished with suitably chosen machinery and methods, and lowest possible cost, in order this to fulfill the basic conditions for an economical burning process.
2- To produce a homogenous mixture which will quickly be converted in the kiln into a homogeneous clinker containing no free lime . As a rule, size reduction raw materials are effected in at least two main stages :
1-crushing (primary reduction) 80 and 20 mm size
2-grinding (fine reduction) 0.2 mm size
3- The capacity of the crusher, reduction ratio, hardness, fragment size, moisture content, plasticity and abrasiveness of the material are important factors affecting the choice of the size reduction machines and methods for dealing with it.
Crushers Type
Hammer Crushers
Impact Crushers
Jaw Crushers
Gyratory Crushers
Roller Crushers
Single – Rotor hammer crusher (O.&K.)
Single Shaft Hammer Crusher
Twin-rotor Hammer Crusher
Grid Bar Cross-Sections
Hammer Crusher with Feed Rollers
Auxiliary Equipment
For Changing worn Parts
Particle Size distribution for hammer crusher product for quarry feed
Hammer Crusher Highlights
Function :Impact & percussive action
Action : Continuos
Reduction ratio : 50:1
Capacity :2000 t/h for the double rotor
Application :Primary reduction of medium hard to hard material
Single Rotor Impact Crusher
Compound Impact Crusher “Hazemag”
Single Impeller crushed-breaker plates & Breaker bars
Impact action of a double Impeller impact
Double Impeller Impact Crusher with Housing
Impact Crusher Highlights
Function Impact surface
Action Continuos
Reduction ratio single crusher 6:1 and 20:1
compound crusher 60:1
Capacity 1500T/h
Application Suited for brittle hard and medium hard material,the single rotor used as primary crusher only .
Toggle Crusher
Single Toggle Jaw Crusher
Double Toggle Jaw Crusher
Jaw crusher highlights
Function Compressive action
Action Intermittent
Reduction ratio 6:1 to 8:1
Capacity Low capacity » 300 T/H
Application Primary crusher for very hard abrasive
materials of low moisture Content,
single toggle crusher is better for
inclusion of stick Materials but, higher
wear than the double toggle.
Gyratory Crusher
Crushing Action of a Gyratory Crusher
Gyratory crusher highlights
Function Compressive action
Action Intermittent
Reduction 12:1 to 15:1
Capacity 6000 T/H
Application
Primary crusher for very hard abrasive material of low moisture
Roller Crusher
Single Roller Crusher
Double Roller Crusher
Product particle size distribution Compression type crusher
Main factors in crusher performance
Impacts r.p.m.
Diameter
Separation between breaker plates
Crushing Plants Stationary Crushing Plants
stationary crushing plant with direct feed dump trucks
Static Primary crushing plant with preliminary screening on stepped (multi-stage) grizzlies
Grizzly with elliptical rotating rollers
Mogensen sizer (illustration of its principle)
Protection against foreign bodies
Metal Detector + magnetic drum separator
Crusher with Dryer
Schematic diagram of typical system
1- Loader
2- Mobile Crushing Installation
3- Travelling Tripper
4- Shiftable belt Conveyor System
5- Stationary Belt Conveyor System
Mobil Crushing plants
Wheel mounted (Rubber tyred) O.&K.
Crawler-mounted
Rail mounted – two sections
Hydraulic walking mechanism O.&K
Lifting Vehicles moving