post #5 Quality KPIs

Previous Post
Next Post

Contents

Quality KPIs

to Download the Book of KPI in cement Industry and more than 12 expert books in cement industry kindly click here 

 

Raw Meal Fineness

Target: To be defined on an individual basis

Purpose: To indicate if the quality parameters for the raw meal production have been achieved consistently

Criteria: Samples are taken according to the sampling plan. The result is calculated for the entire population of samples over the reporting period.

Reporting: Each month for the current production year and the result for the preceding production year

Impact: High standard deviation or average not in target will make burning conditions of the raw mix unstable

Causes of under-performance:

Lack of control
Variable raw materials feed or air flow

Inconsistent raw materials supply

Raw materials are difficult to grind

Separator efficiency
Bad sampling

Kiln Feed Chemistry

Measured for:Blending Silo kiln feed (Lime Saturation Factor, Silica and Alumina Modulus)

Target: To be defined on an individual basis

Purpose: A measure of the control and homogeneity of the production of kiln feed.

Criteria: Samples are taken according to the sampling plan.
The result is calculated for the entire population of samples over the reporting period.

Reporting: Each month for the current production year and the result for the preceding production year

Impact: A high variation in kiln feed chemistry or average not in target causes unsteady kiln operation and high variations in product quality

Causes of under-performance:

Lack of homogenization in the blending silo.

Lack of ratio control in raw meal production

Clinker Chemistry

Measured for:Clinker (C3S and Free Lime)

Target:To be defined on an individual basis

Purpose:Measurement of control of kiln operation and clinker quality

Criteria:

Samples are taken according to the sampling plan.
The result is calculated for the entire population of samples over the reporting period.
C3S is calculated according to the Bogue Formula (see Definitions)

Reporting: Each month for the current production year and the result for the preceding production year

Impact: High variation in clinker chemistry will result in poor product quality

Causes of under-performance:

Unsteady kiln operation
High variation in kiln feed quality

Inconsistent fuel or feed rate to kiln

Uncontrolled addition of filter dust

Wrong kiln parameters

Cement Quality

Measured for: Cement (Fineness in Blaine, Strength at 28 days)

Target:To be defined on an individual basis

Purpose:To measure the variation in finished product quality

Criteria: Samples will be daily composite samples from all hourly process control samples in accordance with sampling plan. Samples must be well homogenized.
The result is calculated for the entire population of samples over the reporting period.

Reporting: Each month for the current production year and the result for the preceding production year

Impact: High variation will result in variable concrete strength and requires higher cement content in concrete.

Causes of under-performance:

Inadequate targets for clinker chemistry
Lack of control of raw meal and clinker production

Lack of control of the cement circuit
Sampling error
Separator efficiency

to Download the Book of KPI in cement Industry and more than 12 expert books in cement industry kindly click here 

Previous Post
Next Post

Leave a Comment

Your email address will not be published. Required fields are marked *

Ask a Cement Engineer ×
Hello! Ask me any cement plant technical question — kiln, grinding, quality, maintenance, preheater. I'll give you a practical answer.