Analysis of Cement Kiln Production Malfunctions and Their Solutions

Previous Post
Next Post

Contents [hide]

Analysis of Cement Kiln Production Malfunctions and Their Solutions

 

TO Download this post and all the books and excel sheets and my personal notes and presentations I collected about cement industry in the last 30 years click the below paypal link 

 

In the cement industry, maintaining the efficiency and reliability of kiln operations is crucial for optimal production. However, several common malfunctions can occur during the kiln’s operation, leading to significant disruptions. This post explores these issues in detail, focusing on their causes, effects, and potential solutions.

1. Grate Jamming in the Cooling Machine

One of the most critical issues faced in cement kiln operations is the jamming of the grate in the cooling machine. The primary cause of this malfunction is the excess material that accumulates in the cooling machine, leading to operational halts. The excess material typically results from several factors:

  1. Kiln Skin or Rear Ring Shedding: The shedding of a large amount of kiln skin or rear ring can cause a significant surge of material into the cooling machine, leading to jamming.
  2. Kiln Burning Issues: Powdered materials can fall into the cooling machine due to burning issues in the kiln. These materials often move slowly, exacerbating the jamming problem.
  3. Excessive Air Blowing: When too much air is blown, it can suspend the dust, which, upon settling, presses down on the bed, causing jamming.

To understand how the grate cooler works under normal conditions, it is essential to recognize that it plays a critical role in the heat exchange process within the cement rotary kiln. The cooler ensures that the clinker temperature rapidly decreases after it falls from the kiln, which is vital for maintaining the system’s efficiency. However, when the cooling process is disrupted by excess material or improper operation, it can lead to severe complications, including the formation of “snowmen” or large clinker balls that can obstruct the cooler and even cause blockages in the clinker crusher.

2. Coal Powder Pipeline Blockage

The transportation of coal powder is another critical area prone to malfunctions. Blockages in the coal powder pipeline can severely impact kiln operations. The causes of such blockages include:

  1. Clogging of the Inlet Filter: The Roots blower, which is essential for transporting coal powder, can suffer from reduced air volume and pressure due to a clogged inlet filter. Regular cleaning of the filter is necessary to prevent this issue.
  2. Loose or Slipping V-Belts: If the V-belts on the blower are loose or slipping, it can result in inadequate air volume, leading to blockages.
  3. Unstable Coal Feeding: Inconsistent feeding of coal can cause an accumulation of excess coal, resulting in pipeline blockages.

Preventative measures include regular maintenance of the blower’s V-belts and inlet filter, along with ensuring stable coal feeding to avoid excessive accumulation in the pipeline.

3. Raw Material Clinkering in the Kiln

Clinkering of raw materials within the kiln is a common issue that can lead to significant operational problems. The primary causes include:

  1. Prolonged Low-Temperature Operation: If the kiln operates at low temperatures for extended periods without proper adjustments, it can lead to raw material clinkering.
  2. Unstable Coal Supply: Poor coal distribution within the kiln can result in low decomposition rates, leading to clinkering.
  3. Kiln Coating or Ring Formation: Significant kiln coating or ring formation can result in an increase in unburnt materials and incomplete combustion, causing clinkering.
  4. Fluctuations in Raw Material Feed Rates: Large fluctuations in feed rates can lead to unpredictable kiln behavior, resulting in clinkering.
  5. Preheater Blockages: Blockages or collapses in the preheater can cause a sudden flow of materials into the burning zone, leading to clinkering.

Addressing these issues requires careful monitoring of kiln temperatures, coal supply stability, and preheater conditions to ensure that the materials are processed correctly and avoid clinkering.

4. Kiln Tripping Causes

Kiln tripping is another significant issue that can disrupt production. The causes of kiln tripping include:

  1. Increased Kiln Filling Coefficient: Slow operation without reducing the material load can result in excessive material in the kiln, leading to tripping.
  2. Significant Kiln Coating or Ring Formation: These issues can cause increased material tumbling inside the kiln, leading to overcurrent tripping.
  3. Excessive Kiln Temperature: High temperatures can cause materials to carry over excessively, contributing to tripping.
  4. Mechanical Faults: Operational strain due to mechanical faults can lead to overcurrent tripping.
  5. Interlocking Stoppages: Automatic tripping can occur due to interlocking stoppages in the system.

To prevent kiln tripping, it is essential to monitor the kiln’s material load, temperature, and mechanical condition continuously.

5. Manual Coal Feeding During Kiln Operation

In situations where the temperature gauge at the outlet of the decomposition furnace is broken, preventing automatic coal feeding, manual feeding becomes necessary. In such cases, it is crucial to rely on the temperatures of other levels to maintain normal operation. Additionally, monitoring the O2 and CO content is essential to determine the appropriate coal feeding rate to avoid disruptions.

6. Kiln Lining Issues During Shutdowns

During planned kiln shutdowns, it is important to ensure that the materials inside the kiln are properly emptied. One common issue that arises is the excessive length of the kiln lining. Proper control of the flame and careful management of the raw material bin and coal powder levels are necessary to avoid difficulties during maintenance.

7. High f-CaO Content in Clinker

High free calcium oxide (f-CaO) content in clinker can lead to quality issues. The causes include:

  1. Poor Homogenization of Raw Materials: Inconsistent raw material mixing can lead to high f-CaO content.
  2. Large Particle Size of Raw Materials: Larger particles may not fully react, leading to high f-CaO levels.
  3. Poor Quality of Coal Powder: Subpar coal powder can result in incomplete combustion, affecting clinker quality.
  4. Unstable Thermal System: Inconsistent kiln temperatures can lead to improper clinker formation.
  5. Excessive Material Layer Thickness: A thick material layer can prevent proper burning, leading to high f-CaO content.
  6. Low Calcination Temperature: Insufficient temperature during calcination can cause incomplete clinker formation.
  7. Improper Coal Injection: Incorrect positioning of coal injection pipes and insufficient primary air volume can lead to poor combustion and high f-CaO content.

To mitigate high f-CaO content, it is essential to maintain consistent raw material mixing, ensure proper coal powder quality, and stabilize the kiln’s thermal system.

8. Clinker Powderization Issues

Powderization of clinker is a problem that can arise due to several factors:

  1. Improper Chemical Composition: Inadequate calcination or coarse fineness of raw materials can lead to high f-CaO content, causing powderization.
  2. Phase Transformation: The transformation of β-C2S to γ-C2S can lead to expansion and powderization.
  3. Non-Uniform Raw Material Composition: Low KH value, high iron content, and excessive liquid phase can lead to clinker powderization due to the formation of FeS and olivine.

Preventing clinker powderization requires attention to the chemical composition of raw materials and ensuring uniform calcination.

Conclusion

Effective management of cement kiln operations requires a deep understanding of the potential malfunctions and their underlying causes. By addressing issues such as grate jamming, coal powder pipeline blockages, raw material clinkering, kiln tripping, and clinker powderization, cement plants can improve their operational efficiency, reduce downtime, and ensure consistent product quality.

Regular maintenance, careful monitoring, and prompt corrective actions are essential to preventing these common kiln malfunctions. By implementing the solutions outlined in this post, cement plants can enhance their overall performance and minimize the risk of disruptions in their production processes.

TO Download this post and all the books and excel sheets and my personal notes and presentations I collected about cement industry in the last 30 years click the below paypal link 

 

 

 