BALL Mill Critical Speed
% Critical speed:
- Practically, mill speed between 68 and 82% of critical speed.
- % critical speed is the mill actual speed in RPM divided by nc.
Example:
3.98 meter mill with rotational speed of 15.6 rpm then nc = 21.2, % critical speed = 73.6 %.