Important operation parameters in Vertical mill

TO DOWNLOAD THE EXCEL SHEET AND ALL THE OTHER USEFUL BOOKS AND RESOURCES KINDLY CLICK HERE 

 

 

  • Feed rate to mill, production rate [t/h].
  • Mill differential pressure [mbar]
  • Grinding bed thickness with span [mm].
  • Amount of external material recirculation [t/h, or BE current A]
  • Gas flow through mill [act. m³/h].
  • Vibration velocity at mill gearbox [mm/s].
  • Power consumption of mill motor with span [kW or alternatively A]
  • Power consumption of system fan [kW]
  • Mill outlet temperature [°C].
  • Tension pressure [bar]
  • Classifier speed [rpm]
  • Fineness of product [Residue on 90µm sieve , Blain, moisture]
  • Amount of water injection [l/h]

 

 

 

 